330 SUH heat-resistant steel
Standard: JIS (G 4311 heat-resistant steel bars)
Grade: SUH 330
â ¢ SUH 330 features and applications.
330 SUH heat-resistant steel, Japan JIS Standard Austenitic Series heat-resistant steel. SUH 330 to 820 to 1150 Degrees C the resistance to oxidation and are of a good than SUH 310 anti-carbon, anti-Nitrided, good, and therefore, heat-resistant strain. Thus, for stove parts and oil decomposition, and so on. 330 SUH corresponding China GB 1 Cr Ni 16 35, the United States ASTM/AISI330/USN N 08,330.
â ¢ SUH 330 chemical composition:
Carbon C: ≤ 0.15
Silicon Si: ≤ 1.50
Manganese Mn: ≤ 2.00
Phosphorus P: =0.040
Sulfur S: =0.030
Chrome Cr: 14.00 - 17.00
Molybdenum Mo: -
Nickel Ni: 33.00 - 37.00
Copper Cu: -